Dear customers,
Currently, the printing and shipping of print documents (standards and regulations) are delayed.
If available, you may also order the document in digital download format; it is usually available within a few minutes (or within one business day at the latest if manual review is required).
To convert an existing order, please email international@dinmedia.de, including your order number or customer number.
We apologize for the inconvenience and thank you for your patience.
Your DIN Media
Standard [CURRENT]
Product information on this site:
Quick delivery via download or delivery service
All transactions are encrypted
This part of ISO 4629 specifies a titrimetric method for determining the free hydroxyl groups in binders and binder solutions for paints and varnishes. The hydroxyl groups may be present as polyhydric alcohols, partial esters, polyester end groups or hydroxylated fatty acids.
This method is not applicable to resins containing both hydroxyl groups and epoxy groups, because the latter will also be included in the result. Also the method is not applicable to cellulose nitrate or to phenolic resins.
The hydroxyl groups contained in a test portion are acetylated with acetic anhydride. The excess acetic anhydride is hydrolysed and the resulting acetic acid is titrated with potassium hydroxide solution, either in the presence of a colour indicator or potentiometrically.
The responsible German standardization committee is Working Committee NA 002-00-02 AA "Lackrohstoffe" ("Raw materials for paints and varnishes") at DIN Standards Committee Coatings and Coating Materials (NAB).
This document replaces DIN EN ISO 4629:1998-07 , DIN 53240-1:2013-06 .